1 Main use
(S) A285A/B/C is used to manufacture structural parts in boilers and pressure vessels.
2 grades and standards
Product grade: (S) A285A/B/C
Executive Standard: ASTM A285/A285M-04 ASME SA285/SA285M-04
3 Technical conditions of supply
3.1 Product Specifications
6~80×1500~4000×Lmm;
3.2 Chemical composition
Table 1 Chemical composition, %
Steel Grade | C | Mn | P | S |
(S)A285A | ≤0.17 | ≤0.90 | ≤0.035 | ≤0.035 |
(S)A285B | ≤0.22 | ≤0.90 | ≤0.035 | ≤0.035 |
(S)A285C | ≤0.28 | ≤0.90 | ≤0.035 | ≤0.035 |
3.3 Mechanical properties table
2 Mechanical properties
Steel Grade | ReL,N/mm2 | Rm,N/mm2 | A200,% |
(S)A285A | ≥165 | 310~450 | ≥27 |
(S)A285B | ≥185 | 345~485 | ≥25 |
(S)A285C | ≥205 | 380~515 | ≥23 |
Normalizing state impact performance:
3.4 Delivery status: hot rolling, normalizing
Steel Grade | Specification,mm | Impact TMCP,℃ | Sample Direction | Acceptance Value,J |
(S)A285A | 6~25 | 4 | Portrait | ≥14 |
>25~80 | 16 | |||
(S)A285B | 6~25 | 10 | ||
>25~80 | 21 | |||
(S)A285C | 6~25 | 16 | ||
>25~80 | 27 |